What surface finishing options are available for CNC machined metal and plastic parts?
The short answer
CNC machined parts can be finished in about a dozen ways, and the substrate narrows the list first. Aluminium takes anodizing in Type II or Type III; steel and stainless take plating, passivation or electropolishing; plastics take bead blasting, vapour smoothing or paint. The function you need, not the look, decides which one.
What a finish actually does to a CNC part
Every finish belongs to one of two families, and knowing which family you are buying explains most of the surprises. A removal finish takes material away: bead blasting, tumbling and electropolishing all change the surface profile and can move a critical dimension, usually by well under 0.01 mm on a blast and by 10 to 40 microns on an electropolish. A build-up finish adds material: anodizing, plating, powder coating and painting all grow the part, and that growth is what breaks tolerances when it was not planned for.
The second distinction is what the finish is for. Corrosion resistance, wear resistance, cleanability, electrical conductivity, adhesion for a later coat, and appearance are six different requirements, and no single finish serves all six. An anodic layer on aluminium protects against corrosion and holds a dye, but it is also an electrical insulator, so it has to be masked off any grounding contact. Powder coating resists impact and ultraviolet light but is thick enough to close a thread. Sorting the requirement first removes most of the options immediately.
Metal finishes by substrate
Aluminium, carbon steel and stainless steel each have a default finish and a set of alternatives, and the substrate decides which ones are physically available. Aluminium cannot be passivated in the stainless sense, stainless steel cannot be anodized, and carbon steel is normally plated or coated because it has no protective oxide of its own.
Aluminium. Anodizing is the default because the process converts the surface into aluminium oxide rather than adding a coating that can flake. Type II sulphuric anodizing builds a 5 to 25 micron layer in clear or a range of dyes. Type III, also called hardcoat, builds 25 to 100 microns and reaches a hardness of 300 to 500 HV, which is the version specified for sliding wear, abrasive exposure and marine hardware. Both are electrical insulators, so a grounding face must be masked or machined after finishing. Powder coating, at 60 to 120 microns cured around 200 degrees Celsius, is the usual choice for housings where colour and impact resistance matter more than dimensional precision.
Carbon steel. Every finish on carbon steel is either a barrier or a sacrificial layer. Zinc plating at 5 to 15 microns protects the steel sacrificially, which is why it is used on bolts, brackets and any part that will be scratched. Electroless nickel at 10 to 25 microns is chosen where a hard, uniform layer is needed on a complex geometry, because it plates evenly inside recesses where electroplating thins out. Powder coating and wet paint are the cheapest routes to a durable colour.
Stainless steel. Stainless is protected by its own chromium oxide layer, so the two finishes that matter most are passivation and electropolishing, and neither is decorative in the ordinary sense. Passivation removes free iron left by machining and restores the oxide layer; it does not change roughness or remove tool marks, which is why specifying it as a cosmetic finish is a common error. Electropolishing goes further, removing 10 to 40 microns of surface and dropping roughness from a machined 1.6 micrometres to roughly 0.4, and that combination of a smooth, chemically clean surface is what makes it the default for pharmaceutical and food-contact parts.
| Finish | Substrate | Thickness effect | Choose it for |
|---|---|---|---|
| As machined | All metals and plastics | None | Internal parts and the tightest dimensions |
| Bead blasting | Metal, hard plastic | Removes a few microns | A uniform matte and a base for coating |
| Type II anodizing | Aluminium, titanium | Adds 5 to 25 microns | Corrosion resistance and colour |
| Type III hard anodizing | Aluminium | Adds 25 to 100 microns | Wear surfaces, 300 to 500 HV |
| Powder coating | Most metals | Adds 60 to 120 microns | Impact, UV stability and colour |
| Zinc or nickel plating | Steel, copper, brass | Adds 2 to 25 microns | Corrosion and electrical contact |
| Passivation | Stainless steel | Effectively none | Free iron removal, food and medical |
| Electropolishing | Stainless steel | Removes 10 to 40 microns | Bright, chemically clean, low Ra |
| Vapour smoothing | ABS, polycarbonate | Removes surface peaks | Gloss on a printed or machined plastic part |
| Painting | All substrates | Adds 20 to 60 microns | Colour and texture on plastic housings |
Plastic parts: what works and what does not
Plastic behaves differently because there is no oxide to grow and no metal to plate. Four finishes cover almost every case. Bead blasting works on hard plastics and gives the same uniform matte as it does on metal, which hides machining marks on a visible face. Vapour smoothing exposes an ABS or polycarbonate surface to solvent vapour, melting the top few microns so the surface flows flat, which can take a printed or machined part from a roughness near 3 micrometres to below 0.5 and give it a gloss that looks moulded rather than machined. Mechanical polishing brings acrylic and polycarbonate to optical transparency, though it is labour-intensive and rarely economic below prototype quantity. Painting, with a primer and a clear coat, is the only practical way to put a durable colour on a plastic part and is common on enclosures and medical housings.
Two limits apply across all four. Plastics are thermal insulators, so a powder coat cured at 200 degrees Celsius is off the table for anything with a low heat-deflection temperature. And the solvents used in vapour smoothing attack some polymer families and not others, so the process is specified by resin rather than by appearance: it suits ABS and polycarbonate and is usually avoided on nylon and acetal.
Every finish moves the part, so plan the 50/50 rule
An anodic oxide grows roughly half into the metal and half out of it. A 20 micron Type II anodize therefore adds about 10 microns to each side, and a 50 micron hard anodize adds about 25. A 20 mm bore specified at plus or minus 0.025 mm and machined to nominal comes out undersized by 25 microns after a heavy anodize, and the part is scrap unless the machinist was told to cut it undersize deliberately. The working rule is to state on the drawing whether the tolerance applies before or after finishing, and to give a pre-finish dimension for every face the finish touches.
Powder coating is less predictable than anodizing and grows a part by 18 to 72 microns per side depending on the gun, the powder and the geometry, which is enough to block a thread that was not plugged. Threads, bearing seats, press-fit bores, sealing faces and conductive contacts need explicit masking, and masking is hand labour, so it is worth designing the part so a simple plug or tape line will do. Plating sits in the middle: electroless nickel at 25 microns grows 25 microns on every surface uniformly, including inside a blind hole, which is an advantage for a wear surface and a problem for a close-fit bore.
Choosing on function rather than appearance
The expensive finishing decisions are the ones made on appearance alone. Naming the function first narrows the field quickly. Corrosion resistance on aluminium means anodizing or a conversion coating, not a bead blast, which is cosmetic only. Wear resistance on a sliding surface means Type III hard anodizing or hard chrome, both of which change dimensions the most and therefore need the pre-finish planning above. Cleanability and low surface energy on stainless means passivation at minimum and electropolishing where the requirement is genuinely hygienic. Electrical conductivity on a housing or bracket means a conversion coating rather than anodizing, because the anodic layer is an insulator and will break a ground path. Adhesion for a later coat means a blast profile, which is why bead blasting and powder coating are usually specified together. And appearance alone, on an indoor part that will not be handled aggressively, is often satisfied by as-machined plus a light blast at a fraction of the cost of anything else.
Where a finish is the wrong specification
Five failures account for most finishing rejections. Specifying the finish after the part has been machined is the first, because there is then no stock allowance for coating growth. Leaving the finish unspecified on the drawing is the second: the shop picks something defensible, the inspector reads it differently, and the argument is unwinnable because nothing was written down. Specifying a Class A cosmetic face without a rack plan is the third, since anodize and plating racks leave contact marks and the requirement cannot be met if the only available contact points land on the visible surface. Treating passivation as a cosmetic finish is the fourth, because it restores corrosion resistance and nothing else. And assuming two finishes are interchangeable because they look alike in a photograph is the fifth: a matte blast and an anodized layer behave completely differently in service.
Two limits close the subject. Every figure here is a planning range for small and medium parts, and the layer a shop actually achieves depends on alloy, bath chemistry, part geometry and the age of the tank, so the only reliable number is a first-article measurement on your own part. And the dimensional figures are nominal rather than guaranteed: an anodize specified at 20 microns still passes at 24, so any tolerance tighter than the coating growth belongs on a masked, machined surface rather than on a coated one.
See surface finishing for the finishes discussed here, CNC machining for the process that makes the base part, and plastic parts for moulded components that are finished the same way.
Scope and sources. The roughness table — as-machined at Ra 1.6 to 3.2 micrometres, bead blasted 0.8 to 1.6, anodized 0.8 to 1.6, Type III hard anodized 0.4 to 0.8, powder coated 1.6 to 3.2, polished 0.1 to 0.4 and electropolished 0.1 to 0.4 — the 50/50 growth rule in which a 25 micron anodize adds 12.5 microns to each side, the powder coat growth of 18 to 72 microns per side, the guidance to highlight masking zones for threads, bearing seats, press-fit bores and mating faces, and the note that tightening Ra from 3.2 to 0.4 can triple cycle time, come from a CNC surface finish guide. The removal-and-build figures — polishing and bead blasting removing up to 0.01 mm, anodizing and plating adding 5 to 150 microns, powder coating adding 50 to 200 microns — the finish table of as-machined 1.6 to 3.2, bead blasted 3.2 to 6.3, anodized 0.8 to 1.6 and polished 0.1 to 0.4 micrometres, and the selection advice by material and by function, come from a surface finishing reference for machined parts. The coating thickness specifications — Type II anodizing 4 to 12 microns, Type III around 50 microns, powder coating 18 to 72 microns cured at 200 degrees Celsius, and electroplated nickel and chrome layers — come from a metal finishing process comparison. The salt-spray and thickness figures for anodizing at 10 to 50 microns and powder coating at 50 to 100 microns come from a surface finishing capability summary. This version replaces the unsourced finishing example and the market figures that appeared in an earlier version of this answer. All figures are planning ranges for small to medium parts; the definitive number for a given part is a first-article measurement after the finish is applied.